Tableros de partículas fabricados con residuos industriales de madera de Pinus patula

Luis Zambrano, Pablo Moreno, Freddy Muñoz, Jorge Durán, Darío Garay, Styles Valero

Producción científica: Contribución a una revistaArtículorevisión exhaustiva

2 Citas (Scopus)

Resumen

This study is a proposal to generate uses of industrial residues from sawmills of Pinus patula wood for the manufacturing of particleboards. The aims are to manufacture homogeneous particleboards with two density levels, determine their physical and mechanical properties and evaluate the results with German and Venezuelan standards. The average water absorption at 2 and 24 hours of both density levels of boards meets the requirements for both standards. The average thickness variation (swelling) by immersion en water at 2 and 24 hours for boards with average density of 767 kg m-3 meets the requirements for both standards. For the case of the panels with average density of 672 kg m-3 thickness variation at 24 hours meets the requirements of both standards, while the swelling at 2 hours does not. Regarding the mechanical properties both the modulus of rupture in static bending and tension perpendicular (internal bond) for both real density levels exceed the minimum accepted by standards, demonstrating that industrial residues from P. patula wood exhibit good technological characteristics for medium density particleboards manufacture.

Título traducido de la contribuciónParticle boards manufactured from industrial residues of pinus patula wood
Idioma originalEspañol
Páginas (desde-hasta)65-80
Número de páginas16
PublicaciónMadera y Bosques
Volumen19
N.º3
EstadoPublicada - 2013

Palabras clave

  • Density
  • Medium density particleboard
  • Perpendicular tension
  • Physical and mechanical properties
  • Static bending