Strengthening via microstructure refinement in bulk Al4 mass% fe alloy using high-pressure torsion

Jorge M. Cubero-Sesin, Zenji Horita

Producción científica: Contribución a una revistaArtículorevisión exhaustiva

22 Citas (Scopus)

Resumen

A bulk Al4 mass% Fe alloy processed by extrusion or by a combination of extrusion and successive annealing was subjected to severe plastic deformation (SPD) through high-pressure torsion (HPT) for up to 75 revolutions. Microstructural evolution was examined by optical microscopy and transmission electron microscopy with special attention for the grain refinement in the Al matrix and for the distribution and morphology of Fe-containing intermetallic particles. Solubility of Fe in the Al matrix was studied by X-ray diffraction (XRD). A significant increase in Vickers microhardness was observed because of the development of an ultrafine-grained matrix and a fine fragmentation of the intermetallic particles especially at an early stage of SPD. The strengthening was affected by the initial state of the microstructure prior to HPT, but finally it was saturated at a higher degree of straining.

Idioma originalInglés
Páginas (desde-hasta)46-55
Número de páginas10
PublicaciónMaterials Transactions
Volumen53
N.º1
DOI
EstadoPublicada - 2012
Publicado de forma externa

Huella

Profundice en los temas de investigación de 'Strengthening via microstructure refinement in bulk Al4 mass% fe alloy using high-pressure torsion'. En conjunto forman una huella única.

Citar esto